Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP KONDUIT OTF2B PPS - Linear LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RL0049S PA 66 LNP LUBRICOMP* RL0049S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Flame Retardant, Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Unnotched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp OFM66 PPS LNP* Thermocomp* OFM66 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP fo.. |
|||
Izod Impact, Unnotched | 1.70 J/cm @Thickness 3.20 mm |
3.18 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |