Material Notes:
LNP* Thermocomp* OFM66 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ASTM D 638
Elongation at Break 2.8 %
2.8 %
ASTM D 638
Flexural Strength 172 MPa
24900 psi
ASTM D 790
Flexural Modulus 17.94 GPa
2602 ksi
ASTM D 790
Izod Impact, Notched 0.370 J/cm

@Temperature 23.0 °C
0.693 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 1.70 J/cm

@Temperature 23.0 °C
3.18 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 276 °C

@Thickness 3.20 mm
529 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 3.20 mm
489 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Dissipation Factor 0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D 150