Polymer Property : Izod Impact, Unnotched = 1.10 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Izod Impact, Unnotched 1.10 - 10.7 J/cm
2.06 - 20.0 ft-lb/in
Average value: 6.54 J/cm Grade Count:14
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda..
Izod Impact, Unnotched 1.10 - 1.30 J/cm
2.06 - 2.44 ft-lb/in
Notch Status Unknown
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver
Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello..
Izod Impact, Unnotched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..