Niche Polymer PPHM6BK Homopolymer PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Niche Polymer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PPHM6BK Homopolymer PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000100 - 0.0200 cm/cm
0.000100 - 0.0200 in/in
ASTM D955
Melt Flow 6.00 g/10 min
6.00 g/10 min
ASTM D123
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 31.0 MPa
>= 4500 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Strength 48.3 MPa
7000 psi
ASTM D790
Flexural Modulus >= 1.24 GPa
>= 180 ksi
ASTM D790
Izod Impact, Unnotched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 119 °C
246 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 160 - 165 °C
320 - 329 °F
ASTM D789
Descriptive Properties Value Comments
Color Black