Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 18.0 MPa @Time 3.60e+6 sec |
2610 psi @Time 1000 hour |
stress leading to 1% elongation; dry; ISO 899-1 |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Creep Strength | 18.0 MPa @Time 3.60e+6 sec |
2610 psi @Time 1000 hour |
stress leading to 1% elongation; dry; ISO 899-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Creep Strength | >= 18.0 MPa | >= 2610 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 18.0 MPa | >= 2610 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Creep Strength | >= 18.0 MPa | >= 2610 psi | 2% elongation, 1000 h; DIN 53444 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |