Creep Strength 18.0 MPa

@Time 3.60e+6 sec
2610 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Creep Strength 18.0 MPa

@Time 3.60e+6 sec
2610 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Creep Strength >= 18.0 MPa
>= 2610 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry
Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH
Creep Strength >= 18.0 MPa
>= 2610 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH
Creep Strength >= 18.0 MPa
>= 2610 psi
2% elongation, 1000 h; DIN 53444
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry
Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH