Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 12.5 J/cm² @Temperature 23.0 °C |
59.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 12.5 J/cm² | 59.5 ft-lb/in² | ISO 179 |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Charpy Impact Unnotched | 12.5 J/cm² | 59.5 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH. |
|||
Charpy Impact Unnotched | 12.5 J/cm² | 59.5 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Charpy Impact Unnotched | 12.5 J/cm² @Temperature -30.0 °C |
59.5 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® X10S 773 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 12.5 J/cm² - NB | 59.5 ft-lb/in² - NB | Average value: 18.9 J/cm² Grade Count:15 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Charpy Impact Unnotched | 12.5 J/cm² | 59.5 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Charpy Impact Unnotched | 12.5 J/cm² @Temperature 30.0 °C |
59.5 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |