BASF Procom® X10S 773 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® X10S 773 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa
2320 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 1.25 GPa
181 ksi
Charpy Impact Unnotched NB
NB
12.5 J/cm²

@Temperature -30.0 °C
59.5 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 95.0 µm/m-°C

@Temperature 20.0 °C
52.8 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Vicat Softening Point 43.0 °C
109 °F