Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²

@Temperature 23.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Charpy Impact Unnotched 0.600 - 1.00 J/cm²
2.86 - 4.76 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Charpy Impact Unnotched 1.00 - 1.00 J/cm²

@Temperature -20.0 - -20.0 °C
4.76 - 4.76 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 1.00 J/cm² Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²

@Temperature 23.0 °C
2.38 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²

@Temperature 23.0 °C
2.38 - 4.76 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Charpy Impact Unnotched 0.800 - 1.00 J/cm²
3.81 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Charpy Impact Unnotched 0.800 - 1.00 J/cm²
3.81 - 4.76 ft-lb/in²
ISO 179
Vyncolit 4221 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group
Charpy Impact Unnotched 0.850 - 1.00 J/cm²
4.05 - 4.76 ft-lb/in²
ISO 179
Vyncolit 4451 XB Novolac Phenolic
Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a..
Charpy Impact Unnotched 0.800 - 1.00 J/cm²
3.81 - 4.76 ft-lb/in²
ISO 179
Vyncolit 2723 W Novolac Phenolic
Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound
UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati..
Charpy Impact Unnotched 0.500 - 1.00 J/cm²
2.38 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
Charpy Impact Unnotched 0.700 - 1.00 J/cm²
3.33 - 4.76 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..