Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, Coloured OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 1.90 J/cm² | 4.76 - 9.04 ft-lb/in² | Average value: 1.48 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 666D Polystyrene
(discontinued **) STYRON® 666D general purpose polystyrene resin is used in injection molding applications, particularly for medical, pharmaceutical and food uses. It offers excellent clarity, intermediate flow char.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Charpy Impact Unnotched | 1.00 - 1.00 J/cm² @Temperature -20.0 - -20.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.00 J/cm² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Charpy Impact Unnotched | 1.00 - 4.00 J/cm² | 4.76 - 19.0 ft-lb/in² | Average value: 3.00 J/cm² Grade Count:38 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² - NB | 4.76 ft-lb/in² - NB | Average value: 3.77 J/cm² Grade Count:30 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed
&nbs Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® Frost 952 51 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants. Very high dimensional stability.Availability: Africa & Middle East; Asia Pa.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latishield 36/AR-10A-V0E ABS, Steel Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Information provided by Lati Indust.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179 |
Vyncolit X689 Novolac Phenolic Glass fiber filled and molybdeendisulfide modified phenolic molding compound with excellent mechanical and thermal properties and lower thermal expansion coefficient. It has excellent friction prop.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided .. |
|||
Charpy Impact Unnotched | 1.00 J/cm² | 4.76 ft-lb/in² | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® C40H 455 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1189 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Charpy Impact Unnotched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
|
BASF Luranyl® KR 2456/3 Polyphenylene Ether + Styrene-Butadiene Blend Heat resistant grade containing halogen-free flame-retardant. Mainly used for functional electronic parts that must meet tough fire-safety legislation.Data was collected by ISO methods and provided.. |
|||
Charpy Impact Unnotched | 1.00 - 4.70 J/cm² @Temperature -20.0 - -20.0 °C |
4.76 - 22.4 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 2.98 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |