Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 - 7.90 J/cm² @Temperature -30.0 - -20.0 °C |
7.14 - 37.6 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.28 J/cm² Grade Count:29 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |