Material Notes:
Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important properties: High stiffnessSpecial UV-stabilizationexcellent surface finishlow warpagenearly isotropic shrinkage These special properties allow the usage of Grilon XE 5004 for parts with high demands for surface quality and direct UV-treatment. Examples are Housings and for example door handles.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 120 MPa
17400 psi
conditioned; ISO 2039-1
175 MPa
25400 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
90.0 MPa
13100 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
9.0 %
9.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 3.70 GPa
537 ksi
conditioned; ISO 527-1/-2
8.50 GPa
1230 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
dry; ISO 179/1eU
6.00 J/cm²
28.6 ft-lb/in²
conditioned; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.600 J/cm²
2.86 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
conditioned; IEC 60243-1
34.0 kV/mm
864 kV/in
dry; IEC 60243-1
Descriptive Properties Value Comments
Automotive Exterior
Form Granules
Industry & Consumer goods Mechanical Engineering
Sports & Leisure
Processing Injection Molding
Special Characteristics Improved UV resistance (outdoor use)
Light stabilized or stable to light