Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® S650FR BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)<

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® S650FR BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)<.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced black flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527-1/-2
Elongation at Break 7.2 %
7.2 %
Nominal; ISO 527-1/-2
Elongation at Yield 4.6 %
4.6 %
ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/-2
Flexural Strength 100 MPa
14500 psi
ISO 178
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.380 J/cm²
1.81 ft-lb/in²
ISO 179/1eA
0.340 J/cm²

@Temperature -30.0 °C
1.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 30 %
30 %
ISO 4589-1/-2
Descriptive Properties Value Comments
Part Marking Code >PBT-FR(17)<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT-FR(17)
UL recognition UL