Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179/1eU |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature -30.0 °C |
24.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-0664 Polyphthalamide, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Grupo Repol Dinalon® B1S25 G30 PA6 30% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179-1 |
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179-1 |
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 5.20 J/cm² @Temperature 23.0 °C |
24.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent .. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® S 4090 GX 14% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179 |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO 179 |
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry) Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability. |
|||
Charpy Impact Unnotched | 5.20 J/cm² | 24.7 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 5.20 - 8.00 J/cm² @Temperature -40.0 - -20.0 °C |
24.7 - 38.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 6.57 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |