Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 20-0664 Polyphthalamide, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Grupo Repol Dinalon® B1S25 G30 PA6 30% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179-1
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Conditioned
Information provided by Unitika Ltd.
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179-1
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry
Information provided by Unitika Ltd.
Charpy Impact Unnotched 5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Rynite® 530 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength stiffness and toughness excellent ..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179 1eU
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT
Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 5.20 - 8.00 J/cm²

@Temperature -40.0 - -20.0 °C
24.7 - 38.1 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.57 J/cm² Grade Count:5
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Copyright © lookpolymers.com All Rights Reserved