Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
ISO 179/1eU
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/2C
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact Unnotched 4.40 J/cm² - NB

@Temperature -40.0 - -20.0 °C
20.9 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 8.98 J/cm² Grade Count:68
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eU
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
Type 1, Edgewise; ISO 179
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eU
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st..
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra..
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
ISO 179
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co..
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin
20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 4.40 J/cm²
20.9 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..
Copyright © lookpolymers.com All Rights Reserved