Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.50 - 16.0 J/cm² | 16.7 - 76.1 ft-lb/in² | Average value: 7.12 J/cm² Grade Count:17 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Charpy Impact Unnotched | 3.50 - 16.0 J/cm² @Temperature -30.0 - 30.0 °C |
16.7 - 76.1 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 7.53 J/cm² Grade Count:12 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Charpy Impact Unnotched | 7.00 - 16.0 J/cm² @Temperature -30.0 - -30.0 °C |
33.3 - 76.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 10.2 J/cm² Grade Count:9 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 6.50 - 16.0 J/cm² @Temperature -40.0 - -20.0 °C |
30.9 - 76.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 9.56 J/cm² Grade Count:11 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |