Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15315 NC010 PBT
(Unverified Data**) Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature 23.0 °C |
2.95 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® CE15315 NC010 PBT
(Unverified Data**) Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature 23.0 °C |
2.95 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE30-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon
(Unverified Data**) Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by Du.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature 23.0 °C |
2.95 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-GM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Charpy Impact, Notched | 0.620 J/cm² @Temperature -30.0 °C |
2.95 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A 35E 990 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |