DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon
Manufacturer DuPont Performance Polymers
Trade Name Zytel® PLUS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Thickness 2.00 mm
0.0040 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Thickness 2.00 mm
0.0070 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa

@Temperature 23.0 °C
20000 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 2.6 %

@Temperature 23.0 °C
2.6 %

@Temperature 73.4 °F
DAM; ISO 527
Tensile Modulus 7.35 GPa

@Temperature 23.0 °C
1070 ksi

@Temperature 73.4 °F
DAM; ISO 527
Flexural Strength 197 MPa

@Temperature 23.0 °C
28600 psi

@Temperature 73.4 °F
DAM; ISO 178
Flexural Modulus 6.50 GPa

@Temperature 23.0 °C
943 ksi

@Temperature 73.4 °F
DAM; ISO 178
Charpy Impact Unnotched 3.60 J/cm²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eU
3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.620 J/cm²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
0.640 J/cm²

@Temperature 23.0 °C
3.05 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 237 °C
459 °F
DAM; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 0.810 mm
V-0

@Thickness 0.0319 in
DAM; IEC 60695-11-10
Processing Properties Metric English Comments
Melt Temperature 285 °C
545 °F
DAM; Optimum
275 - 295 °C
527 - 563 °F
DAM
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
100 °C
212 °F
DAM; optimum
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Forms Pellets
DAM
Generic Nylon
DAM
Material Status Preliminary Data
DAM
Part Marking Code >PA-GF15FR(17)<
ISO 11469; DAM
Processing Method Injection Molding
DAM
Product Category Flame Retardant Resins
DAM
Glass Reinforced Resins
DAM
SHIELD Technology Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA-GF15FR(17)
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM