Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.20 J/cm² @Temperature 20.0 °C |
10.5 ft-lb/in² @Temperature 68.0 °F |
ISO 179/1eA |
Polyplastic Armlen® PP GF 20-1EX Polypropylene Copolymer, 20% Glass Fiber Information provided by PolyPlastic Group. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV330 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S 35HR (cond.) Nylon 6 PA6 medium-high viscosity injection molding grade. Easy mould release.Information provided by Radici group. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 179-1eA |
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66 PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® E309 ABS Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C (1984) |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/2 |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene Saxalac 835U is an antistatic, easy flowing light stabilized ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical prop.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K-FG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K-FHG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |