Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs XX0 ABS, Extrusion Grade Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -20.0 °C |
10.5 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 45H PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV330 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax BTE70-FN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Novodur® E309 ABS Novodur E309 is a extrusion grade especially designed for furniture profilesInformation provided by Styrolution |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Styrolution Novodur® P2M-V ABS Pellets Novodur® P2M-V has high impact strength, high gloss, and low emission. It is used for the production of molded plastic articles. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C (1984) |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/2 |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/2 |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber A chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® K224-PG2 PA6-I-GF8 8% Glass Reinforced, Impact Modified |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6
(Unverified Data**) Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR30 NL IH PA 6.6 30% glass fiber reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |