Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.Characteristics of Arnitel:Excellent strength over a wide range of temperaturesExcellent dynamic properties e.g. creep and fatigueHigh heat resistanceExceptional resistance to oils and greasesGood chemical resistanceHigh degree of versatility in processingEasy coloring using masterbatchesSurface quality from high gloss to texturedExcellent heat resistance (long term 165°C)Good electrical insulation propertiesLow moisture absorption, excellent dimensional stabilityEasy flow, fast cooling timesTypical Applications: Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in consumer electronic companies. Arnitel® is a good choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.Information provided by DSM.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 3.5 %
3.5 %
Similar to ISO 62
Moisture Absorption at Equilibrium 0.40 %
0.40 %
Similar to ISO 62
Melt Flow 34.75 g/10 min

@Load 2.16 kg,
Temperature 240 °C
34.75 g/10 min

@Load 4.76 lb,
Temperature 464 °F
Calculated from 25cm3/10min volume-flow rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
3 seconds; ISO 868
Tensile Strength at Break 21.3 MPa
3090 psi
ISO 527-1/-2
Tensile Strength, Yield 7.90 MPa

@Strain 5.00 %
1150 psi

@Strain 5.00 %
ISO 527-1/-2
10.6 MPa

@Strain 10.0 %
1540 psi

@Strain 10.0 %
ISO 527-1/-2
14.1 MPa

@Strain 50.0 %
2050 psi

@Strain 50.0 %
ISO 527-1/-2
16.1 MPa

@Strain 100 %
2340 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 235 %
235 %
ISO 527-1/-2
Tensile Modulus 0.240 GPa
34.8 ksi
ISO 527-1/-2
Charpy Impact, Notched 2.20 J/cm²

@Temperature -30.0 °C
10.5 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
6.00 J/cm²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
IEC 60695-11-10