Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT Polyamide 6 FeaturesBasic type PA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical .. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NGR PA6, basic type FeaturesPA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, faste.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-5120 BLH 20% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5120 BLH is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/.INNOPOL® CS 1-5120 BLH is recommended especially for producing products, where high stiffn.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 0.000 °C |
0.761 ft-lb/in² @Temperature 32.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® BB 75 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -20.0 °C |
0.761 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® GB 802 Polypropylene Random Copolymer Applications include injection molding and extrusion. Basic stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -20.0 °C |
0.761 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® MT 805 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -20.0 °C |
0.761 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Unipetrol PP MONSTEN® FC 908 Polypropylene Random Copolymer Applications include injection molding and packaging films. Slip and antiblocking agent stabilization. Random copolymer.Information provided by Unipetrol RPA |