Unipetrol PP MONSTEN® GB 802 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Unipetrol RPA
Trade Name PP MONSTEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PP MONSTEN® GB 802 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications include injection molding and extrusion. Basic stabilization. Random copolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Break >= 250 %
>= 250 %
ISO 527
Flexural Modulus 0.950 GPa
138 ksi
ISO 178
Charpy Impact, Notched 0.160 J/cm²

@Temperature -20.0 °C
0.761 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ISO 75
Vicat Softening Point 132 °C
270 °F
ISO 306