Material Notes:
Applications include injection molding and packaging films. Slip and antiblocking agent stabilization. Random copolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 250 %
>= 250 %
ISO 527
Flexural Modulus 0.800 GPa
116 ksi
ISO 178
Charpy Impact, Notched 0.160 J/cm²

@Temperature -20.0 °C
0.761 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ISO 75
Vicat Softening Point 132 °C
270 °F
ISO 306