Polymer Property : Izod Impact, Notched = 5.60 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.149 - 2.99 J/cm
0.280 - 5.60 ft-lb/in
Average value: 0.785 J/cm Grade Count:43
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Izod Impact, Notched 0.350 - 2.99 J/cm

@Temperature -40.0 - -40.0 °C
0.656 - 5.60 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.52 J/cm Grade Count:12
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched 0.320 - 2.99 J/cm
0.600 - 5.60 ft-lb/in
Average value: 0.842 J/cm Grade Count:15
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..