Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.1 MPa
7700 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 68.97 MPa
10000 psi
ASTM D790
Flexural Modulus 2.589 GPa
375.5 ksi
ASTM D790
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 123.89 °C
255.00 °F
ASTM D648