Polymer Property : Izod Impact, Notched = 19.9 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.427 - 10.6 J/cm
0.800 - 19.9 ft-lb/in
Average value: 3.59 J/cm Grade Count:12
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..