Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.427 - 10.6 J/cm | 0.800 - 19.9 ft-lb/in | Average value: 3.59 J/cm Grade Count:12 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |