Aclo Accucomp Polycarbonate POL051L Medium Viscosity

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polycarbonate POL051L Medium Viscosity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
MD; ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength at Break 69.98 MPa
10150 psi
ASTM D638
Tensile Strength, Yield 69.98 MPa
10150 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Elongation at Yield 105 %
105 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 97.97 MPa
14210 psi
ASTM D790
Flexural Modulus 2.699 GPa
391.5 ksi
ASTM D790
Izod Impact, Notched 9.02 J/cm
16.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F