Material Notes:
UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
DIN 53479
Water Absorption 0.023 - 0.026 %
0.023 - 0.026 %
DIN 53495
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ASTM-D638
Elongation at Break 120 %
120 %
ASTM-D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM-D790
Izod Impact, Notched 9.00 J/cm

@Temperature 23.0 °C
16.9 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm
635 kV/in
VDE 0303/4
Copyright © lookpolymers.com All Rights Reserved