Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AN16L-53 Polypropylene, Compounded Description: Compounded polypropylene produced for automotive exterior applications using Mytex® Technology.Key Applications: Body side moldingInformation provided by Mytex Polymers |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS65KWLGUS Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene with high stiffness, superior impact balance, surface hardness and extremely low gloss.Key Applications: Non-painted instrument panelInformation pro.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific) Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5211 PC+ABS (Asia Pacific) CY5211 is a FR PC+ABS of non-brominated, non-chlorinated flame retardant systems with balanced flow, impact and hydrolytic stability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific) Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific) Standard Flow OQ Resin |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® OQ1022 PC (Europe-Africa-Middle East) Standard Flow OQ Resin |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature -30.0 °C |
10.3 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature -30.0 °C |
10.3 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched | 5.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.3 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL FW-715C Friction and Wear Resistant POM, Polymeric Wear Additive, CaCo3 Filled, Low Warpage, Antistatic LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 5.49 J/cm | 10.3 ft-lb/in | |
Kuraray SEPTON® CM2 Compatibilizer Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A60N02 Nylon 66, Chemically Coupled 60% Long Fiber A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 6600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | >= 5.50 J/cm | >= 10.3 ft-lb/in | LAB034 |
ExxonMobil Mytex™ AN17K-01 Rubber modified polypropylene for automotive interior applications.Information provided by ExxonMobil Chemical |
|||
Izod Impact, Notched | 5.50 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.3 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABSPC 7801 ABS/PC Injection Molding Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.50 J/cm @Temperature -30.0 °C |
10.3 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers Tekaloy® G70A4 Impact Resistance at Low Temperature PC/ABS Alloy Impact Resistance at Low TemperatureInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 5.50 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.3 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABSPC 7801E ABS/PC Extrusion Grade, High Impact, High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |