Material Notes:
Description: Compounded polypropylene produced for automotive exterior applications using Mytex® Technology.Key Applications: Body side moldingInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 20
20
ASTM D785
Tensile Strength, Yield 16.0 MPa
2320 psi
50 mm/min; ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 5.50 J/cm

@Temperature 23.0 °C
10.3 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648