Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256-93a
Multibase Multi-Pro® 2005 XRC Black 20% Filler Content Polypropylene
Multi-Pro 2005 XRC is specifically designed for injection molded electronic industrial uses. This product shows higher heat distortion and notched izod than typical glass filled polypropylene. Thi..
Izod Impact, Notched 0.609 J/cm
1.14 ft-lb/in
ASTM D256
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement  (discontinued **)
ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data ..
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256
Kolon KOCETAL® K500 Standard Grade Acetal Resin
General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon.
Izod Impact, Notched >= 0.610 J/cm
>= 1.14 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Karina E 830-35/1-Y-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles/.p>Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.610 J/cm
>= 1.14 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Karina E 832-35/1-Y-ERA-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.610 J/cm
>= 1.14 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Karina E 832-35/1-Y-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.610 J/cm
>= 1.14 ft-lb/in
Reversed Notch (Method E); ASTM D 256
Karina E 834-35/1-Y-ERA-LMP Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256-93a
Multibase Multi-ABS 8933 Black
Ash is 28% per ASTM D-5630-94.Data provided by Multibase.
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU
LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant.
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT
LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66
LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized.
Izod Impact, Notched 0.609 J/cm
1.14 ft-lb/in
Tra-Con Tra-Bond FS163 Medium Viscosity Epoxy/Polyamide Adhesive
TRA-BOND FS163 is a medium viscosity polyamide/epoxy adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are r..
Izod Impact, Notched 0.609 J/cm
1.14 ft-lb/in
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive
TRA-BOND 2143D is a medium viscosity adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This tw..
Izod Impact, Notched 0.608 J/cm
1.14 ft-lb/in
ASTM D256
Cheng Yu Plastic PP237G2 Polypropylene, 20% Glass Fiber
Izod Impact, Notched 0.609 J/cm

@Temperature 22.8 °C
1.14 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Ensinger TECANYL™ MT CF30 Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
Izod Impact, Notched 0.608 J/cm
1.14 ft-lb/in
ASTM D256
Cheng Yu Plastic A708G3 SAN, 30% Glass Fiber
Izod Impact, Notched 0.610 J/cm
1.14 ft-lb/in
ASTM D256
Plenco 51015 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..