Material Notes:
TRA-BOND FS163 is a medium viscosity polyamide/epoxy adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This two-part adhesive is easily mixed and cured at room temperature, and develops strong bonds to most clean, dry material surfaces including most metals, rigid plastics, glass, ceramics, leather, rubber, wood and concrete. Fully cured TRA-BOND FS163 bonds offer good low temperature electrical, mechanical, and impact resistant properties, superior thermal shock resistance, low permeability to gases and vapors, good dimensional stability, and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis, and many other chemicals.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 30000 cP

@Temperature 25.0 °C
30000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Izod Impact, Notched 0.609 J/cm
1.14 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 64.0 µm/m-°C

@Temperature 20.0 °C
35.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 3.35

@Frequency 1000 Hz
3.35

@Frequency 1000 Hz
Dielectric Strength 18.1 kV/mm
460 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 75 min
75 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/100
Resin/Hardener