Mechanical Properties Metric English Comments
Izod Impact, Notched 0.160 - 0.907 J/cm
0.300 - 1.70 ft-lb/in
Average value: 0.527 J/cm Grade Count:4
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..
Izod Impact, Notched 0.590 - 0.907 J/cm

@Temperature -40.0 - -40.0 °C
1.11 - 1.70 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.730 J/cm Grade Count:3
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..