Material Notes:
Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 22 g/10 min

@Load 3.80 kg,
Temperature 230 °C
22 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.9 MPa
5210 psi
ASTM Data
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM Data
Elongation at Break 20 %
20 %
ASTM Data
Tensile Modulus 2.41 GPa
350 ksi
ASTM Data
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM Data
Impact Test 20.9 J

@Temperature 23.0 °C
15.4 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.8 °C
199 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM Data
Vicat Softening Point 107 °C
225 °F