Material Notes:
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc

@Temperature 22.8 °C
1.05 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 93.1 MPa
13500 psi
Max Load; ASTM D790
Flexural Modulus 3.65 GPa
530 ksi
secant; ASTM D790
5.48 GPa
795 ksi
tangent; ASTM D790
Izod Impact, Notched 0.694 J/cm

@Temperature 22.8 °C
1.30 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
305 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Users viewing this material also viewed the following: