Material Notes:
Description: SEQUEL® E2200 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require low-temperature toughness and high rigidity. This product is fully colorable and is available in both UV-stabilized and non-UV-stabilized options. It is most functional when used as substrate layer for INDURE® E1500HG to provide a structure with excellent cold temperature impact properties as well as high stiffness. Applications: Substrate layer for E1500HG high gloss cap layer or general purpose monolith material for sheet extrusion and thermoforming. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
ASTM D955
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 210 %
210 %
ASTM D638
Flexural Modulus 1.379 GPa
200.0 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
NB; ASTM D256
0.694 J/cm

@Temperature -30.0 °C
1.30 ft-lb/in

@Temperature -22.0 °F
PB; ASTM D256
Gardner Impact >= 36.2 J

@Temperature -30.0 °C
>= 26.7 ft-lb

@Temperature -22.0 °F
ASTM D5420-96
>= 36.2 J

@Temperature 23.0 °C
>= 26.7 ft-lb

@Temperature 73.4 °F
ASTM D5420-96
Thermal Properties Metric English Comments
CTE, linear 81.2 µm/m-°C

@Temperature 20.0 °C
45.1 µin/in-°F

@Temperature 68.0 °F
modified; ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 HB