Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ATH-25GF-10MN/000 Acetal-Homopolymer, Glass/Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass/Mineral ReinforcedChemically CoupledInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 107 MPa
15500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 176 MPa
25500 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.614 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.15 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257