Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Ovation Polymers
Trade Name Nima™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nima™ HL 30530 GF FR PET, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PET – Flame Retardant 30% Short Glass Fiber Reinforced. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.69 g/cc
1.69 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 115 MPa
16700 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Tensile Modulus 6.00 GPa
870 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 168 MPa
24400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.614 J/cm
1.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0