Material Notes:
Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers.
Physical Properties Metric English Comments
Melt Flow 2.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength at Break 70.3 MPa
10200 psi
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
ASTM D790
Izod Impact, Notched 0.246 J/cm
0.460 ft-lb/in
0.250 inches; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
Unannealed; 0.250 inches; ASTM D648
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Flammability, UL94 HB
HB
0.125 inch