Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade

Category Polymer , Thermoplastic
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-transparent, natural, medium impact resistance, high hardness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 2.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength, Ultimate 70.3 MPa
10200 psi
ASTM D638
Flexural Yield Strength 118 MPa
17100 psi
ASTM D790
Flexural Modulus 3.727 GPa
540.5 ksi
ASTM D790
Izod Impact, Notched 0.246 J/cm
0.460 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C
187 °F
ASTM D648
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified