Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.118 - 1.47 J/cm | 0.220 - 2.76 ft-lb/in | Average value: 0.297 J/cm Grade Count:163 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.118 J/cm | 0.220 ft-lb/in | ASTM D256 |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where.. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C.. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond F118 Fiber Optic Epoxy Adhesive TRA-BOND F118 is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows mor.. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows .. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity.. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Tra-Con Tra-Bond F131 High Tg Room Temperature Cure Fiber Optic Adhesive TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus .. |
|||
Izod Impact, Notched | 0.117 J/cm | 0.220 ft-lb/in | |
Atom Adhesives AA-BOND F131 Epoxy Adhesive AA-BOND F131 is two parts fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. AA-BOND F131 produces a typical .. |