Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond F113SC BLK High Tg Fiber Optic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND F113SC BLK is a fiber optic adhesive used for terminating ALL types of fiber optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus meeting specification requirements of BELLCORE and connector manufacturers. This two-part, low viscosity system can be cured at room temperature overnight or as fast as 8 minutes at 90°C. Its black color allows for easy polishing. TRA-BOND F113SC BLK has a useable WORKING LIFE in FIBER OPTIC applications of 20 minutes. It is also excellent for small potting and sealing applications where the WORKING LIFE is 2 hours. This 100% solid system has excellent resistance to impact and thermal shock. F113SC BLK is supplied in 2 gram (or larger) BIPAX kits, PRE-MIXED and FROZEN syringes or 1 gram MINIPAX.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
Mixed
Viscosity 2200 cP

@Temperature 25.0 °C
2200 cP

@Temperature 77.0 °F
Mixed (rv #4, 20 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Adhesive Bond Strength 25.5 MPa
3700 psi
Lap shear, alum to alum
Izod Impact, Notched 0.117 J/cm
0.220 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 95.0 °C
203 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1080 min

@Temperature 25.0 °C
18.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
25 grams
Descriptive Properties Value Comments
Color Black
Mix Ratio, parts by weight 100/28
Resin/Hardener
Thixotropic Index 1
5 rpm/50 rpm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved