Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.600 - 8.50 J/cm² | 2.86 - 40.5 ft-lb/in² | Average value: 5.66 J/cm² Grade Count:27 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 4.50 - 8.50 J/cm² | 21.4 - 40.5 ft-lb/in² | DIN 53453 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Charpy Impact, Notched | 0.300 - 8.50 J/cm² @Temperature -40.0 - -20.0 °C |
1.43 - 40.5 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.86 J/cm² Grade Count:56 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.300 - 8.50 J/cm² | 1.43 - 40.5 ft-lb/in² | Average value: 1.41 J/cm² Grade Count:9 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |