Polymer Property : Charpy Impact, Notched = 7.40 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific)
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Partial Break
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned)
Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM)
Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding
Charpy Impact, Notched 7.40 J/cm²
35.2 ft-lb/in²
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding