Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 20% Glass Fiber Reinforced
Manufacturer Addiplast
Trade Name Addinyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Conditioned; ISO 868
84
84
ISO 868
Tensile Strength at Break 80.0 MPa
11600 psi
Conditioned; ISO R 527
130 MPa
18900 psi
ISO R 527
Elongation at Yield 4.0 %
4.0 %
ISO R 527
10 %
10 %
Conditioned; ISO R 527
Modulus of Elasticity 3.00 GPa
435 ksi
Conditioned; ISO 178
5.50 GPa
798 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
11.0 kJ/m²
5.23 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/IeU
5.50 J/cm²
26.2 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/IeA
0.800 J/cm²
3.81 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C
19.4 µin/in-°F
ASTM E831
Melting Point 243 °C
469 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1
32.0 kV/mm
813 kV/in
CEI 60243-1
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A