Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 - 0.750 J/cm²

@Temperature 23.0 °C
2.38 - 3.57 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Charpy Impact, Notched 0.0600 - 0.750 J/cm²

@Temperature -30.0 - -20.0 °C
0.286 - 3.57 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.489 J/cm² Grade Count:8
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact, Notched 0.450 - 0.750 J/cm²
2.14 - 3.57 ft-lb/in²
Average value: 0.650 J/cm² Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 0.350 - 0.750 J/cm²

@Temperature -30.0 - -20.0 °C
1.67 - 3.57 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.550 J/cm² Grade Count:2
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Charpy Impact, Notched 0.750 - 0.750 J/cm²

@Temperature -30.0 - -30.0 °C
3.57 - 3.57 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.750 J/cm² Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..