Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 0.750 J/cm² @Temperature 23.0 °C |
2.38 - 3.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.0600 - 0.750 J/cm² @Temperature -30.0 - -20.0 °C |
0.286 - 3.57 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.489 J/cm² Grade Count:8 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact, Notched | 0.450 - 0.750 J/cm² | 2.14 - 3.57 ft-lb/in² | Average value: 0.650 J/cm² Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact, Notched | 0.350 - 0.750 J/cm² @Temperature -30.0 - -20.0 °C |
1.67 - 3.57 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.550 J/cm² Grade Count:2 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Charpy Impact, Notched | 0.750 - 0.750 J/cm² @Temperature -30.0 - -30.0 °C |
3.57 - 3.57 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.750 J/cm² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |